Table 1 X-ray diffraction peak parameters of biosynthesized Nanogold using Coleus forskohlii leaf extract (CFLE) as a green reducing and capping agent.
2theta | HKL | FHWM | Grain size | Assignment |
|---|---|---|---|---|
38.50 | 111 | 0.228 | 36.89 | Most intense peak; dominant facet in fcc gold nanoparticles |
43.61 | 200 | 0.167 | 51.39 | Secondary intense reflection |
64.42 | 220 | 0.108 | 86.63 | Higher-order reflection |
77.63 | 311 | 0.168 | 60.70 | Confirms fcc lattice symmetry |
Average crystallite size | 58.90 | |||