Table 1 2PP processing parameters.
From: Fabrication of biodegradable drug-eluting scaffolds by two-photon polymerization
Process parameter | Value | Unit |
|---|---|---|
layer thickness | 0.4 | \(\upmu\)m |
Hatch distance | 0.4 | \(\upmu\)m |
Microscope objective field of view | 1000 x 1000 | \(\upmu\)m |
Average laser power (non-degradable photoresist) | 40 | mW |
Average laser power (degradable photoresist) | 70 | mW |
Laser scan speed (non-degradable photoresist) | 50 | mm/s |
Laser scan speed (degradable photoresist) | 300 | mm/s |