Table 1 EDX composition analysis of PmAP, \(\:\text{P}\text{m}\text{A}\text{P}/{\text{G}\text{O}}_{\left(6.6\right)}\), and \(\:\text{P}\text{m}\text{A}\text{P}/\text{A}\text{P}\text{T}\text{E}\text{S}{/\text{G}\text{O}}_{\left(6.6\right)}\:\)

From: Fabrication of a poly(m‑aminophenol)/3-aminopropyl triethoxysilane/graphene oxide ternary nanocomposite for removal of Cu(II) from aqueous solution

Sample

C

wt %

N

wt %

O

wt %

Si

wt %

Cl

wt %

S

wt %

\(\:\text{P}\text{m}\text{A}\text{P}\)

60.61

13.86

15.69

--

4.39

6.45

\(\:\text{P}\text{m}\text{A}\text{P}{/\text{G}\text{O}}_{\left(6.6\right)}\)

41.46

9.81

46.69

0.40

1.64

--

\(\:\text{P}\text{m}\text{A}\text{P}/\text{A}\text{P}\text{T}\text{E}\text{S}{/\text{G}\text{O}}_{\left(6.6\right)}\)

42.14

8.36

30.98

18.39

0.13

--