Table 15 Fitting results of dry shrinkage of inorganic binder stabilized materials with different ratios.
From: Research on the properties of polymer stabilized coal gangue materials in rubber powder slag base
Peer group | Fitting equation | R2 |
|---|---|---|
CS | \(y=177.76\left(1-{e}^{\left(\frac{-x}{9.14}\right)}\right)-14.458\) | 0.9956 |
GSS1 | \(y=18.80\left(1-{e}^{\left(-\frac{x}{40.86}\right)}\right)+94.02\left(1-{e}^{\left(-\frac{x}{5.63}\right)}\right)-12.923\) | 0.9943 |
GSS2 | \(y=42.273\left(1-{e}^{\left(-\frac{x}{4.05}\right)}\right)+90.786\left(1-{e}^{\left(-\frac{x}{11.93}\right)}\right)-1\) 1.309 | 0.9975 |
GSS3 | \(y=50.995\left(1-{e}^{\left(-\frac{x}{14.15}\right)}\right)+108.130\left(1-{e}^{\left(-\frac{x}{5.70}\right)}\right)-14.952\) | 0.9985 |
GSS4 | \(y=81.852\left(1-{e}^{\left(-\frac{x}{4.73}\right)}\right)+106.959\left(1-{e}^{\left(-\frac{x}{13.72}\right)}\right)-16.401\) | 0.9972 |
GSS5 | \(y=79.237\left(1-{e}^{\left(-\frac{x}{4.12}\right)}\right)+128.628\left(1-{e}^{\left(-\frac{x}{12.80}\right)}\right)-18.385\) | 0.9967 |
GSG15-3 | \(y=159.201\left(1-{e}^{\left(\frac{-x}{9.88}\right)}\right)-2.452\) | 0.9977 |
GSG30-3 | \(y=69.396\left(1-{e}^{\left(-\frac{x}{11.26}\right)}\right)+115.489\left(1-{e}^{\left(-\frac{x}{15.67}\right)}\right)-11.548\) | 0.9966 |
GSG45-3 | \(y=206.751\left(1-{e}^{\left(\frac{-x}{10.363}\right)}\right)-\) 10.472 | 0.9968 |