Table 17 Fitting results of drying shrinkage strain of inorganic binder stabilized materials with different ratios.
From: Research on the properties of polymer stabilized coal gangue materials in rubber powder slag base
Peer group | Fitting equation | R2 |
|---|---|---|
CS | \(y=46.192\left(1-{e}^{\left(-\frac{x}{7.43}\right)}\right)-5.368\) | 0.9883 |
GSS1 | \(y=5.303\left(1-{e}^{\left(-\frac{x}{58.38}\right)}\right)+25.211\left(1-{e}^{\left(-\frac{x}{4.59}\right)}\right)-4.812\) | 0.9827 |
GSS2 | \(y=11.552\left(1-{e}^{\left(-\frac{x}{18.42}\right)}\right)+23.565\left(1-{e}^{\left(-\frac{x}{4.62}\right)}\right)-4.476\) | 0.9910 |
GSS3 | \(y=36.059\left(1-{e}^{\left(-\frac{x}{5.04}\right)}\right)+6.570\left(1-{e}^{\left(-\frac{x}{30.89}\right)}\right)-6.022\) | 0.9914 |
GSS4 | \(y=15.844\left(1-{e}^{\left(-\frac{x}{20.92}\right)}\right)+34.372\left(1-{e}^{\left(-\frac{x}{4.59}\right)}\right)-6.686\) | 0.9881 |
GSS5 | \(y=36.609\left(1-{e}^{\left(-\frac{x}{4.40}\right)}\right)+18.271\left(1-{e}^{\left(-\frac{x}{19.05}\right)}\right)-4.582\) | 0.9885 |
GSG15-3 | \(y=22.614\left(1-{e}^{\left(-\frac{x}{4.64}\right)}\right)+20.422\left(1-{e}^{\left(-\frac{x}{14.16}\right)}\right)-3.033\) | 0.9924 |
GSG30-3 | \(y=14.012\left(1-{e}^{\left(-\frac{x}{18.84}\right)}\right)+35.316\left(1-{e}^{\left(-\frac{x}{5.26}\right)}\right)-5.648\) | 0.9871 |
GSG45-3 | \(y=31.016\left(1-{e}^{\left(-\frac{x}{5.39}\right)}\right)+24.111\left(1-{e}^{\left(-\frac{x}{15.089}\right)}\right)-5.756\) | 0.9976 |