Table 4 Performance test results of fly ash.
From: Research on the properties of polymer stabilized coal gangue materials in rubber powder slag base
Test parameters | Test results | Specification requirements |
|---|---|---|
Fineness (%) | 9.2 | ≤ 12 |
Water demand ratio (%) | 91 | ≤ 105 |
Water content (%) | 0.3 | ≤ 1 |
Loss on ignition (%) | 3.01 | ≤ 5 |
Average particle size (µm) | 20.05 | / |