Fig. 5

(a,b) Digital photos for the glycerin-in-styrene derived polymeric monoliths stabilized with 1–5 wt% OCMNs. (c) FTIR spectra of glycerin-in-styrene derived polymeric monolith stabilized with 5 wt% OCMNs, compared to OCMNs. (d) EDX Analysis for glycerin-in-styrene derived polymeric monolith stabilized with 5 wt% OCMNs.