Table 1 Magnetic parameters were obtained at 25 °C for the polymer monolith with 5% OCMNs as a stabilizer.

From: Fabrication of well-defined magnetic microporous polymeric monoliths using simple non-aqueous emulsification technique

Parameter

Value

Area-total

1227 erg/g

Coercivity (Hc)

5.8834 G

Flatness

1.3244

Hc, Negative

− 2.4897 G

Hc, Positive

9.2772 G

Magnetization (Ms)

10.653 emu/g

Mr, Negative

− 0.37486 emu/g

Mr, Positive

9.96E−02 emu/g

Ms, Negative

− 10.743 emu/g

Ms, Positive

10.563 emu/g

Retentivity (Mr)

0.23725 emu/g

Squareness

2.23E−02