Table 1 Average results of concrete test22.
From: Utilizing recycled glass powder in reinforced concrete beams: comparison of shear performance
Test No | Compressive Strength | Splitting Tensile Str. | Flexural Str. |
|---|---|---|---|
REF | 18.89 | 1.33 | 6.26 |
C10% | 18.20 | 1.29 | 5.89 |
C20% | 17.11 | 1.25 | 5.62 |
C30% | 10.67 | 0.99 | 5.24 |