Table 4 Mixture proportions of GGBS/SF-based geopolymer concrete mixtures (kg/m3).
From: Effect of blending GGBS and silica fume on the mechanical properties of geopolymer concrete
Group | Mix Designation | Binder | Dune sand | Coarse Aggregates | AAS ratio | AAS | SP | Water | |||
|---|---|---|---|---|---|---|---|---|---|---|---|
GGBS | SF | 10-mm | 20-mm | SS | SH | ||||||
A | G100S0-A1.5 | 300 | 0 | 725 | 360 | 840 | 1.5 | 36 | 24 | 12 | 100 |
G75S25-A1.5 | 225 | 75 | 725 | 360 | 840 | 36 | 24 | 12 | 100 | ||
G50S50-A1.5 | 150 | 150 | 725 | 360 | 840 | 36 | 24 | 12 | 100 | ||
G25S75-A1.5 | 75 | 225 | 725 | 360 | 840 | 36 | 24 | 12 | 100 | ||
G0S100-A1.5 | 0 | 300 | 725 | 360 | 840 | 36 | 24 | 12 | 100 | ||
B | G100S0-A2.0 | 300 | 0 | 725 | 360 | 840 | 2.0 | 27 | 18 | 12 | 100 |
G75S25-A2.0 | 225 | 75 | 725 | 360 | 840 | 27 | 18 | 12 | 100 | ||
G50S50-A2.0 | 150 | 150 | 725 | 360 | 840 | 27 | 18 | 12 | 100 | ||
G25S75-A2.0 | 75 | 225 | 725 | 360 | 840 | 27 | 18 | 12 | 100 | ||
G0S100-A2.0 | 0 | 300 | 725 | 360 | 840 | 27 | 18 | 12 | 100 | ||