Table 8 TSSR properties of all compounds.

From: Effect of devulcanized reclaimed rubber content on structure, mechanical properties, and thermo-oxidative aging behavior of ethylene-propylene-dien-monomer (EPDM) rubber

Parameter

Crosslink density [mol/m³]

σ0 [MPa]

T50 [°C]

Reference

114

0.47

188.6

20% Devulcanized EPDM

n. a.

0.56

180.9

40% Devulcanized EPDM

n. a.

0.55

166.8

60% Devulcanized EPDM

n. a.

0.59

155.6

60% Devulcanized EPDM with recipe adjustment

n. a.

0.48

165.1