Fig. 15
From: Sustainable activated carbon from palm waste for aqueous nickel II adsorption

pH effect regarding Ni(II) adsorption onto PFTAC (initial concentration = 50 ppm, PFTAC dose = 0.5 g/250 ml, stirring speed = 300 rpm T = 25 ℃ and time = 90 min).