Table 1 Detailed experimental conditions of the STF.
From: Polishing dental ceramics using shear-thickening slurry
Groups | Conditions | Parameters(by weight) |
|---|---|---|
1 | Shear-thickening fluid | Distilled water: Starch = 45:55 |
2 | STF added 500# SiC abrasives | Distilled water: Starch: SiC = 45:50:5 |
3 | STF added 1000# SiC abrasives | Distilled water: Starch: SiC = 45:50:5 |
4 | STF added 2000# SiC abrasives | Distilled water: Starch: SiC = 45:50:5 |
5 | Distilled water: Starch: SiC = 40:50:10 |