Table 2 Mechanical properties of different ratios of Gd2O3/HDPE composites before and after argon ion irradiation.
Sample | Young’s modulus (N) | Tensile Stress (MPa) | elongation percentage @ break (%) |
|---|---|---|---|
HDPE before | 181 | 5.73 | 168.35 |
HDPE after | 78 | 4.53 | 124.82 |
20% Gd before | 38 | 6.08 | 21.33 |
20% Gd after | 30 | 5.81 | 70.06 |
12% Gd before | 53 | 5.6 | 35.94 |
12% Gd after | 41 | 5.92 | 64.19 |