Table 4 Charpy impact test results.

From: Recycling paper waste into structural cellulose composites with enhanced mechanical and thermal performance

Pattern

Dimensions of the fracture site

K

KT

KTśr

S

Thickness

Width

A

[C.M]

[mm]

[mm]

[mm2]

[J]

[kJ/m2]

[kJ/m2]

[kJ/m2]

10.1

7.65

11.54

88.28

0.445

5.041

4.857

0.382

10.2

7.64

11.23

85.80

0.379

4.417

10.3

7.63

11.28

86.07

0.440

5.112

20.1

7.03

11.07

77.82

0.290

3.726

4.262

0.758

20.2

6.61

9.90

65.44

0.314

4.798

20.3

8.53

10.64

90.76

0.293

3.228

30.1

7.42

10.71

79.47

0.404

5.084

4.524

0.493

30.2

7.23

10.69

77.29

0.321

4.153

30.3

7.45

10.71

79.79

0.346

4.336

40.1

7.81

10.66

83.25

0.391

4.696

4.859

0.386

40.2

7.72

10.66

82.30

0.377

4.581

40.3

7.61

10.66

81.12

0.430

5.301

50.1

7.43

10.78

80.10

0.329

4.108

4.243

0.119

50.2

7.44

10.80

80.35

0.348

4.331

50.3

8.12

10.82

87.86

0.377

4.291