Table 6 Characteristic points of TG and DTG graphs from TGA examination.

From: Recycling paper waste into structural cellulose composites with enhanced mechanical and thermal performance

Cellulose content

Amount of material remaining

Fastest weight loss

Temp. of fastest weight loss

(%)

(%)

(%/min)

(°C)

10%

20.54

− 8.24

344.0

20%

23.99

− 6.34

337.1

30%

23.96

− 6.10

336.3

40%

26.83

− 5.61

332.6

50%

9.18

− 6.17

329.3