Table 3 Mix proportions of the LC3 concrete (kg/m3).

From: Impact of construction and demolition wastes on the performance of sustainable LC3-based structural lightweight concrete

Mix Groups

Mixes

Binder

Aggregates

W

SP

AEA

OPC

MK

CBP

LSP

RCP

CBFA

CBCA

Control

C

450

-

-

-

-

544

816

185

6.75

-

L

MKL-30

225

135

-

90

-

544

816

185

6.75

1.125

MKL-40

180

180

-

90

-

544

816

185

6.75

1.125

CBL-30

225

-

135

90

-

544

816

185

6.75

1.125

CBL-40

180

-

180

90

-

544

816

185

6.75

1.125

R

MKR-30

225

135

-

-

90

544

816

185

9

1.125

MKR-40

180

180

-

-

90

544

816

185

9

1.125

CBR-30

225

-

135

-

90

544

816

185

9

1.125

CBR-40

180

-

180

-

90

544

816

185

9

1.125