Table 1 BO and NBOs in AQ glass and HT-6h samples.
From: Transparent ferroelectric glass–ceramics for wastewater treatment by piezocatalysis
Sample | BO peak position (eV) | NBO peak position (eV) | \(\frac{{{\mathbf{NBO}}}}{{{\mathbf{BO}}}}\) (area ratio) |
|---|---|---|---|
AQ-glass | 532.95 | 531.69 | 9.69 |
HT-6h | 532.9 | 531.123 | 2.61 |