Fig. 7: NO release from non-calcinated and calcinated stainless steel and steillite wires. | Communications Materials

Fig. 7: NO release from non-calcinated and calcinated stainless steel and steillite wires.

From: Nitric oxide-generating metallic wires for enhanced metal implants

Fig. 7

Cumulative NO generation after incubating 5 non-calcinated or calcinated a stainless steel or b stellite wires in 200 μL of 50 μM GSNO in PBS over a 24 h time period at 37 °C. Cumulative NO generation after incubating 5 non-calcinated or calcinated c stainless steel or d stellite wires in 200 μL of 0, 12.5, 25, 50, 100, or 200 μM GSNO in PBS over a 24 h time period at 37 °C. Cumulative NO generation after incubating 5 non-calcinated or calcinated e stainless steel or f stellite wires in 200 μL of 50 μM DPTA NONOate, DETA NONOate, NOC-5, β-gal NONOate, or SNAP in PBS over a 0.5 h time period at 37 °C. n ≥ 3; error bars represent standard deviation.