Table 2 Curie (Tc) and melt (Tm) temperatures, melting enthalpy (\({\triangle H}_{f}\)), and crystallinity percentage (\({\chi }_{c}\)), determined from the DSC results for the neat polymer and composites
Sample | Tc (± 0.05 °C) | Tm (± 0.05 °C) | \({\triangle H}_{{{{\rm{f}}}}}\) (± 0.1 J/g) | \({\chi }_{{{{\rm{c}}}}}\) (± 0.1%) |
|---|---|---|---|---|
P(VDF-TrFE) | 101.89 | 151.12 | 22.1 | 24.2 |
CFO5 | 101.72 | 150.62 | 20.3 | 23.4 |
CFO10 | 101.86 | 150.32 | 21.5 | 26.11 |
CFO20 | 102.16 | 149.76 | 15.2 | 20.8 |
CFO20NP | 93.96 | 140.75 | 13.8 | 18.8 |
FO20 | 101.56 | 150.67 | 14.2 | 19.4 |
Nd20 | 101.36 | 150.49 | 16.5 | 22.6 |
NFM20 | 102.20 | 150.44 | 11.5 | 15.7 |
NZFO20 | 101.17 | 150.94 | 15.6 | 21.3 |