Fig. 5: NMR spectra of experimental products containing apatite.

Experiments were conducted at 1300 °C except for the bottom three experiments that were conducted at 1150 °C. Addition of an iron source to a mixture of apatite (Apa), silica (SiO2), and carbon black (CB) produced several reduced and some polymerized P species.