Table 1 Characterization of nickel powder

From: Feasibility of on-site generated nitrogen as a sustainable cold spray process gas

 

Average Moisture Content (ppm)

Average Oxygen Content (ppm)

Average Nitrogen Content (ppm)

Average Hydrogen Content (ppm)

Average Nanohardness (GPa)

Average Modulus (GPa)

Average

64.51

362.67

0.00

13.67

3.02

128.47

STDEV

1.45

5.51

0.00

0.58

0.22

25.64