Figure 4

Comparison of recycling over 3.0%Ru-OMC in this study (a) with various reported metal catalysts4 (b) for LA hydrogenation.
Reaction conditions: LA 5.0 g, catalyst amount 0.3 wt%, H2 pressure 4.5 MPa, temperature 150°C and duration 2 h.

Comparison of recycling over 3.0%Ru-OMC in this study (a) with various reported metal catalysts4 (b) for LA hydrogenation.
Reaction conditions: LA 5.0 g, catalyst amount 0.3 wt%, H2 pressure 4.5 MPa, temperature 150°C and duration 2 h.