Table 2 Tensile and three-point bending properties of rolled WZC alloy at various temperatures
Properties | RT | 100 °C | 150 °C | 200 °C | 300 °C | 400 °C | 500 °C |
|---|---|---|---|---|---|---|---|
Ultimate tensile strength (MPa) | 991 | 1058 | 986 | 963 | 683 | 619 | 582 |
Elongation to failure (%) | 1.1 ± 0.4 | 2.7 ± 1.0 | 6.5 ± 1.3 | 14.2 ± 4.2 | 21.3 ± 2.8 | 27.2 ± 3.2 | 41 ± 5.0 |
Bending strength (MPa) | 2514 | 2266 | 2114 | 2436* | 2156* | 1965* | 1743* |
Yield strength (MPa) | 2086 | 1815 | 1717 | 1344 | 1184 | 1035 | 968 |