Figure 1
From: Disentanglement of growth dynamic and thermodynamic effects in LaAlO3/SrTiO3 heterostructures

Sheet resistances of LAO/STO heterostructures deposited with T = 700 °C and pO2 = 1 × 10−4 mbar.
The samples were post-annealed at 700 °C in varying pO2 for one hour.