Table 1 Summary of the oxidation peak currents and potentials for the detection of AA, DA and UA obtained by CV and DPV employing the OLC electrodes.

From: Inherently-Forced Tensile Strain in Nanodiamond-Derived Onion-like Carbon: Consequences in Defect-Induced Electrochemical Activation

Analyte

Electrode material

CV: Individual detection (1 mM)

CV: Simultanous detection (0.33 mM, respectively)

DPV: Simultanous detection (0.33 mM, respectively)

IP(μA)

EP(V)

IP(μA)

EP(V)

IP(μA)

EP(V)

AA

OLC-1000

5

0.110

2

0.110

0.3

0.024

OLC-1100

30

−0.018

10

0.019

0.5

−0.011

OLC-1200

41

−0.055

15

−0.032

20

−0.054

OLC-1400

42

−0.053

15

−0.015

21

−0.047

DA

OLC-1000

44

0.275

15

0.286

10

0.165

OLC-1100

55

0.219

20

0.212

30

0.170

OLC-1200

112

0.210

38

0.207

220.5

0.169

OLC-1400

109

0.209

37

0.208

217.5

0.173

UA

OLC-1000

32

0.410

12

0.412

12

0.35

OLC-1100

43

0.355

20

0.362

22

0.319

OLC-1200

143

0.346

50

0.349

197.5

0.331

OLC-1400

143

0.355

53

0.352

195.1

0.335