Table 1 Refinement parameters of SrZrO3: 2 mol% Eu3+.
Sample | SrZrO3: 2%Eu3+ |
|---|---|
Crystal Syntem | Orthorhombic |
Space Group | Pnma |
a | 8.208 Å |
b | 8.208 Å |
c | 8.196 Å |
volume | 552.175 (Å)3 |
α=β=γ | 90° |
Rwp | 9.67 |
Rp | 8.16 |
Re | 6.4 |
Sample | SrZrO3: 2%Eu3+ |
|---|---|
Crystal Syntem | Orthorhombic |
Space Group | Pnma |
a | 8.208 Å |
b | 8.208 Å |
c | 8.196 Å |
volume | 552.175 (Å)3 |
α=β=γ | 90° |
Rwp | 9.67 |
Rp | 8.16 |
Re | 6.4 |