Table 1 List of xylan dissolution and cellulose deploymerization fitting parameters to Eqs (2) and (4), respectively.

From: Understanding Longitudinal Wood Fiber Ultra-structure for Producing Cellulose Nanofibrils Using Disk Milling with Diluted Acid Prehydrolysis

Eq. (2)

Eq. (4)

Unit

α = 8.21

None

β = 20.7

L/mol

Ea = 25000

J/mol

θ = 0.623

θ’ = 0.838

None

f = 0.049

f’ = 0.020

None