Figure 5
From: Crystallization and hardening of poly(ethylene-co-vinyl acetate) mouthguards during routine use

Solid-state CP/MAS 13C NMR spectra of (a) EVA28_1 and (b) EVA28_2 before (black) and after (red) repeated compression cycles (10,000 times at 6.0 MPa).