Degradation of heterogeneous catalysts limits their cost efficiency and sustainability. Here a hydrogenation catalyst that is stable over a hundred cycles of reuse is reported, with stability attributed to the formation of an agglomeration at the palladium/silicon interface.
- Yoichi M. A. Yamada
- Heeyoel Baek
- Yasuhiro Uozumi