Table 1 Structures of vinyl-functionalized solvent moieties and textural parameters of the corresponding porous polymeric solid solvents (PSSs).
From: Creating solvation environments in heterogeneous catalysts for efficient biomass conversion
Monomer | PSS | BET surface area (m2 g−1) | Pore volume (cm3 g−1) |
|---|---|---|---|
a | PSS-IL | 460 | 0.60 |
b | PSS-NMP | 596 | 0.53 |
c | PSS-DMSO | 233 | 0.54 |