Table 1 Ethylene polymerization results in toluenea

From: Uniform shape monodisperse single chain nanocrystals by living aqueous catalytic polymerization

Entry (cond.)

Precatalyst

T [C°]

Yield [g]

TOFb

Mnc [103 g mol−1]

Mw/Mnc

Tmd [°C]

Crystallinityd [%]

Branches/1000 Ce

1A

2/Pyr

30

2.21

31.5

275

1.5

133

48

2.8

2B

2/Pyr

50

2.87

136.4

27

1.7

121

47

9.1

3C

2/Pyr

70

0.17

16.2

8

2.0

114

47

14.0f

4A

1-C4F9/Pyr

30

3.60

51.4

489

1.5

133

58

0.8

5B

1-C4F9/Pyr

50

6.43

305.6

305

1.3

131

49

2.2

6D

1-C6F13/Pyr

15

5.26

6.3

1190

1.3

136

49

n.d.

7A

1-C6F13/Pyr

30

5.13

73.2

844

1.5

134

56

0.7

8B

1-C6F13/Pyr

50

8.17

388.4

308

1.4

131

46

1.9

9C

1-C6F13/Pyr

70

8.00

760.6

33

1.6

125

50

6.5

10A

1-C8F17/Pyr

30

3.52

50.2

515

1.5

135

60

0.7

11B

1-C8F17/Pyr

50

3.83

182.1

218

1.5

132

46

1.7

  1. aPolymerization conditions: (A) 5 µmol precatalyst, 30 -min reaction time, (B) 3 µmol precatalyst, 15 min reaction time, (C) 3 µmol precatalyst, 7.5 min reaction time, (D) 5 µmol precatalyst, 5 h reaction time; all experiments performed in 100 mL of toluene with 40 bar ethylene pressure; bgiven in 103 x mol [C2H4] x mol−1 [Ni] x h−1. cDetermined by GPC at 160 °C in trichlorobenzene. dDetermined by DSC with 10 K min−1 heating rate (data from second heating cycle). eDetermined by 13C NMR spectroscopy. fIncluding 2.3 ethyl branches