Fig. 3: Morphology evolution of the prepared Zn anodes.
From: Revealing the role of crystal orientation of protective layers for stable zinc anode

SEM and the corresponding EDX mapping images of a–f ZF@F-TiO2 and g–l ZF@C-TiO2 before and after 10 cycles in Zn-SS cells. Scale bar: 40 μm.