Fig. 4: Thermal stability of cell components and their mixtures in the Gr|NMC811 battery. | Nature Communications

Fig. 4: Thermal stability of cell components and their mixtures in the Gr|NMC811 battery.

From: Thermal runaway of Lithium-ion batteries employing LiN(SO2F)2-based concentrated electrolytes

Fig. 4

a DSC traces of the lithiated anode, concentrated LiFSI/DMC electrolyte components, and their mixtures for the Gr|NMC811 battery. The inset displays the enlarged peaks of An and An + DMC. b NO2 (m/z = 46) gas evolution of LiFSI, the lithiated anode and their mixture during the DSC measurement. c SO2 (m/z = 64) gas evolution of LiFSI, the lithiated anode, and their mixture during the DSC measurement. d The weight loss of the lithiated anode, LiFSI, and their mixture. e DSC traces of the cathode, cathode mixed with concentrated LiFSI/DMC, and cathode mixed with anode.