Table 1 Thermal runaway features of the partial cells and full cell.
From: Thermal runaway of Lithium-ion batteries employing LiN(SO2F)2-based concentrated electrolytes
Cells | Mass (g) | T1 (°C) | T2 (°C) | T3 (°C) | ΔT (°C) | (dT/dt)max (°C S−1) | QTR (kJ) | ΔTeq (°C) |
|---|---|---|---|---|---|---|---|---|
CaEly | 13.9 | 220.3 | – | 288.3 | 68 | – | 0.8 | 37.4 |
AnEly | 13.9 | 130.1 | 202.5 | 712.2 | 582.1 | 882.9 | 7.0 | 312.6 |
CaAn | 17.5 | 140.7 | 225.1 | 724 | 583.3 | 164 | 11.3 | 507.9 |
Full cell | 24.5 | 135.3 | 200.5 | 652.2 | 516.9 | 401.2 | 11.5 | – |