Table 1 Sheet resistance (Rsh), Thickness and Conductivity of different PEDOT:PSS film.

From: Ultra-conformal skin electrodes with synergistically enhanced conductivity for long-time and low-motion artifact epidermal electrophysiology

Methods

Rsh (Ω/sq)

Thickness (nm)

Conductivity (S/cm)

Application

Reference

Ionic liquid additive

59

3100

Stretchable circuit

Sci. Adv. 3, e1602076 (2017)

H2SO4 soaking

46

4000

Solar cell

Adv. Mater. 27, 2317–2323 (2015)

HNO3 soaking

27

4100

Solar cell

Adv. Electron. Mater. 1, 1500121 (2015)

Zn(TFSI)2 doping

4115

Solar cell

Joule 3, 2205–2218 (2019)

MSA soaking

50

79

2540

Solar cell

ACS Appl. Mater. Interfaces 7, 15314−15320 (2015)

Methanol/MSA soaking

43

65

3560

Solar cell

ACS Appl. Mater. Interfaces 7, 16287−16295 (2015)

PTG

45

80

2850

Electrophysiology detection

This work

24

100

4142