Fig. 3: Thermal properties of BoL-LC. | Nature Communications

Fig. 3: Thermal properties of BoL-LC.

From: Liquid crystalline 2D borophene oxide for inorganic optical devices

Fig. 3

a DSC curves corresponding to cooling and heating of BoL-LC. BoL-LC transitions from the P-i to the P-ii phase at ~100 °C during cooling and from the P-ii to the P-i phase at approx. 150 °C during heating. The P-i (b) and P-ii (c) phases in a glass capillary observed by polarized optical microscopy under crossed polarizers (white double arrows) at room temperature. d X-ray diffraction (XRD) peaks of the sample at room temperature (blue). The spectra in gray show peaks calculated from the obtained single-crystal data of BoL-C.