Fig. 4: Comparison of electrochemical properties between W11 and WA111 alloys. | Nature Communications

Fig. 4: Comparison of electrochemical properties between W11 and WA111 alloys.

From: Towards development of a high-strength stainless Mg alloy with Al-assisted growth of passive film

Fig. 4

a Potentiodynamic polarization (PDP) curves for W11 and WA111 alloys after soaking for 1.5 h; b Nyquist plots from electrochemical impedance spectroscopy (EIS) for W11 and WA111 alloys after soaking for 1.5 h; c Nyquist plots from EIS for the as-cast (F) WA111 alloy after soaking for different times. The fitting lines of these Nyquist plots are also listed above.