Fig. 1: In situ XRD analyses of CsxFA1-xPbI3 PQDs.
From: Thermal tolerance of perovskite quantum dots dependent on A-site cation and surface ligand

a In situ XRD patterns collected from 30 °C to 500 °C under argon flowing for FAPbI3, Cs0.25FA0.75PbI3, Cs0.5FA0.5PbI3, Cs0.75FA0.25PbI3, and CsPbI3 PQDs. b Scheme for the dominant reflections in the thermal degradation of CsxFA1-xPbI3 PQDs that are drawn from the in situ XRD data taken at the 2θ angles shown in Supplementary Table 1 for perovskite in QD form (PVK-QDs, red color shading), perovskite in bulk form (PVK-bulk films, solid dark-red color shading), orthorhombic non-perovskite (non-PVK yellow phase, orange color shading), and PbI2 (yellow color shading). The peak of substrate is marked with asterisks. Source data are provided as a Source Data file.