Table 1 Rietveld refinement results of XRD patterns of ZC-67nm and ZC-177μm
From: Single-crystal ZrCo nanoparticle for advanced hydrogen and H-isotope storage
Sample | Lattice constant of ZrCo phase (Å) | Cell volume of ZrCo phase (Å3) | Phase abundance (wt.%) | |||
|---|---|---|---|---|---|---|
ZrCo | ZrCo2 | Zr3Co | ZrH2 | |||
ZC-67nm | 3.195 | 32.605 | 95.5 | 3.3 | 1.2 | 0 |
ZC-177μm | 3.203 | 32.860 | 90.3 | 8.1 | 0 | 1.6 |