Fig. 3: Pit at a slag after open circuit potential testing in 0.6 M NaCl. | Nature Communications

Fig. 3: Pit at a slag after open circuit potential testing in 0.6 M NaCl.

From: Critical role of slags in pitting corrosion of additively manufactured stainless steel in simulated seawater

Fig. 3: Pit at a slag after open circuit potential testing in 0.6 M NaCl.The alternative text for this image may have been generated using AI.

a, b Scanning electron microscopy (SEM) images of a same pitted slag obtained with secondary electrons and back-scattered electrons, respectively. c SEM energy dispersive X-ray spectroscopy of the regions highlighted with the red, dashed square in (b).