Fig. 3: Electrochemical performance and Ex-situ sXRD measurement. | Nature Communications

Fig. 3: Electrochemical performance and Ex-situ sXRD measurement.

From: Efficient direct repairing of lithium- and manganese-rich cathodes by concentrated solar radiation

Fig. 3

The charge-discharge profiles of LMRO-50C (a) and LMRO-50CS (b) electrode. The cycling performance at C/2 (c) and rate capability (d) for LMRO and LMRO-50CS. e Ex-situ sXRD of LMRO-50C and LMRO-50CS samples at representative voltage with the enlarged view in the range of 2Theta = 17.5-20° and 25-35°, and the corresponding selected voltage stages in the first cycle profiles. The (CC) in a–c represents the Charging state and the (DC) represents the Discharging state. 1 C = 250 mAh g−1.