Fig. 7: The performance of ASSLMBs.
From: Deciphering the critical role of interstitial volume in glassy sulfide superionic conductors

a The configuration of the Li | C:G = 7 | NCM83125 full cell. b Cycling performances of Li | Li5.4PS4.4Cl1.6 | NCM83125 and Li | C:G = 7 | NCM83125 full cells at 0.25 mA cm−2. A current density of 0.125 mA cm−2 was applied to activate the full cell for the first 3 cycles. c The voltage profiles of Li | C:G = 7 | NCM83125 full cell at different cycles. d The summary of cycling performance of reported high-voltage ASSLMBs. See Table S10 for detailed reference of each point.