Fig. 5: Recovery of adhesive strength of a damaged interface.
From: Photo-modulated activation of organic bases enabling microencapsulation and on-demand reactivity

a Schematic of lap shear test. A-EA capsules and epoxy capsules are ruptured between two glass slides to initiate adhesive strength. b Time-dependent shear strength development at various temperatures. Data are presented as mean values  ±  SD (n = 3 independent samples).