Table 1 Thermodynamic parameters for protium/deuterium absorption and desorption of ZrCo alloy
From: Isotope engineering achieved by local coordination design in Ti-Pd co-doped ZrCo-based alloys
Parameters | Absorption | Desorption | ||
|---|---|---|---|---|
Q = H | Q = D | Q = H | Q = D | |
ΔH (kJ·mol−1 Q2) | −85.93 | −88.50 | 86.00 | 87.60 |
ΔS (J·K−1·mol−1 Q2) | −141.93 | −147.85 | 126.15 | 129.87 |
T1 bar (°C) | / | / | 408.73 | 401.52 |
Tcr (°C) | 161.12 | 157.11 | ||
Tgap (°C) | / | 251.62 | ||