Fig. 6: Polarized light microscopy images of PEDOT crystal domains (reddish color).

Right- (a) and left-tilted (b) growth of PEDOT crystal domains. Magnification: 145 ×; substrate: SiO2 wafer; film thickness = 32 nm; Scale bar = 190 μm.