Fig. 6: Electrochemical performance of LPSC and UDSH@LPSC samples after 1 day of 33%RH air exposure.

Voltage profiles of a an Li0.5In | LPSC 1D air|LPSC | NCM811 composite cell, and c an Li0.5In | UDSH@LPSC 1D air|LPSC | NCM811 composite cell at 60 °C and at a 0.15 mA cm−2. b, d 50 cycle capacity retention for the cells shown in a and c, respectively. Source data are provided as a Source Data file.