Table 1 Selected examples of photocatalytic degradation of dyes by MOFs and P-containing materials
Catalyst | Catalyst concentration g/L | Dye* | Oxidant | Time | Conversion % | |
|---|---|---|---|---|---|---|
P8-MFM-300 | 0.5 | 10 mg/L RhB | Air | 150 min | 90 | This work |
P8-MFM-300 | 0.5 | 10 mg/L MO | Air | 300 min | 90 | This work |
Milled red phosphorus (RP-36) | 0.4 | 10 mg/L RhB | Air | 6 hours | 88 | |
Bulk black phosphorus | 1.0 | 2·10-4 mg/L MO | Air | 120 min | 25 | |
Black phosphorus nanosheets @ Graphene Oxide | 1.0 | 2·10-4 mg/L MO | Air | 120 min | 100 | |
nMLM | 0.1 | 50 mg/L RhB | 1 ml H2O2 | 240 min | 92 | |
MIL-53-Fe | 0.01 | 4·10-4 M MB | Air | 1 h | 11 | |
UiO66 | 0.1 | 20 mg/L MO | Air | 0 | ||
UiO66-1.25Ti | 1.0 | 10 mg/L MB | Air | 80 min | 82 | |
HKUST-1 | 0.125 | 25.28 mg/L RB13 | Air | 14 h | 40 | |
MIL-100 (Fe) | 0.3 | 5 ppm MO | Air | 7 h | 64 | |
Au@MIL-100(Fe) | 0.125 | 0.02 g/L MO | 10 mM H2O2 | 1.57 h | 100 | |
(Fe-Ti)-(MOF-NH2) (3:1) | 0.1 | 0.05 g/L OrangeII | 14 mM H2O2 | 10 min | 100 | |
(Fe3O4)-(MIL-88B (Fe)) | 0.2 | MB/ RhB 0.1:0.01 mM | 20 mM H2O2 | 1.33 h | 100 | |
MIL88(Fe) | 0.4 | 10 mg/L RhB | 20 mM H2O2 | 80 min | 50 | |
Bi2O3 – Cu-MOF | 1.0 | 10 mg/L RhB | Air | 60 min | 44 | |
Bi2O3 – Cu-MOF– Graphene Oxide (BCG-2) | 1.0 | 10 mg/L RhB | Air | 60 min | 80 |