Fig. 3: Mechanical properties of LLST.
From: Nature-inspired hierarchical building materials with low CO2 emission and superior performance

a Flexural strength of LLST after 28 days of curing. The error bars in Fig. 3. a, b represented the standard deviation, calculated based on three replicate experiments. b Specific compressive strength and c comparison with reported foam cement9,32. d Strain-compressive stress curve of LLST. e Crack propagation was inhibited by pore deformation. f Schematic diagram of multi-scale stress dispersion.