Fig. 6: Electrochemical performance of full cells at 60 °C. | Nature Communications

Fig. 6: Electrochemical performance of full cells at 60 °C.

From: Architected continuum mixed ionic and electronic conducting alloy negative electrode for fast-charging all-solid-state lithium batteries

Fig. 6: Electrochemical performance of full cells at 60 °C.

a Cross-sectional SEM image of the initial InSnBi|LiPSCl|LiCoO2 configuration. b Charging and discharging profiles of InSnBi | |LiCoO2 full-cell from 0.2 C to 6 C (with a fixed discharge rate of 0.5 C and a 3-min constant-voltage charging). c Comparison of the specific power of the InSnBi | |LiCoO2 cell with reported ASSLBs. d Cycling performance of our home-made InSnBi | |LiCoO2 pouch cell (3.5 cm × 5.0 cm) at 4.0 C (The capacity of 53 mAh was measured at a rate of 0.2 C). e The comparison of fast-charging capability between our InSnBi | |LiCoO2 cell and representative publications. (LiCoO2 based on 1 C = 145 mAh g−1).